Chrome Ore Beneficiation Plant

Chrome Ore Beneficiation Plant

As the important part of chrome ore beneficiation plant is designed to provide the most effective pool area and overflow velocity requirements. According to the theory that the deposition rates are quite different because of different solid particles' specific gravity, the chrome ore beneficiation plant is not only able to clean the ground mineral ore, but also separate the particles briefly.Different grains have different specific gravity and sedimentation rates in liquid. This product allows the fine ore to flow in the water, while coarse ore sinks to the bottom. This classifier can filter materials and send coarse materials to the feeding mouth and discharge fine materials from the pipe.

Chrome ore dressing process

The size of raw ore is 340mm. Though two-stage crushing, the size of crushed raw ores can reach 100mm to be screened. The ores whose size is between 100mm and 10mm can be processed by heavy medium separation to get parts of ore concentrate, using two-stage drum cobber. The fine crushed ores whose size is under 10mm will be mixed with the raw ores whose size is under 10mm to be screened. These ores whose size is between 10mm and 0mm, can be classified into continuous grain levels: 10-3mm,3-0mm, then come into jigger to go through jig dressing. In jigger, the ore production will be ground until the size will reach 0.5-0mm and then will be selected by spiral concentrator. All the ore mud will be mixed together then be separated by shaking table.

Chrome Ore Beneficiation Plant foe sale

Ore fine after grinding will expected to enter the next process: classification. Spiral classifier with principle of that different proportion of solid particles in the liquid precipitation different speeds, to wash the mixture of ore, grading. After washing and grading of mineral mix when passing magnetic separator,because of the susceptibility of various minerals is different , through magnetic and mechanical forces to separated the magnetic material from the mixture. After initial separation of mineral particles in the separator is fed to the flotation machine, according to the different characteristics put into different drugs minerals, making the minerals to be separated with other substances. After the minerals to be separated, because they contain large amounts of water,so they must be initially concentrated by the concentrator, and then dried by the dryer, and dried to obtain minerals. Finally, copper concentrate grade of 45%.